I was using solder with a flux core. What i did was tin both sides, crimp wires with needle nose, heat assembly. If I started with too much solder on the pin side from tinning, it would form a small nodule that prevented the pin from locking. What I learned was make sure the wire was not engaged too far and use solder sparingly. I consider my skills with a soldering to be poor...
Tom
tomahawk is offline   Reply With Quote
 

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On

Forum Jump


All times are GMT -8. The time now is 08:25 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
© 2002 Big Water's Edge. All rights reserved.