Old 12-14-2014, 09:09 PM   #8
grey zone
Senior Member
 
Join Date: Mar 2005
Location: san diego
Posts: 158
I use Classic Coat which comes in 4oz. bottles and if I did not have that I would use Flex Coat. The pot lives of the two are similar and after about 20 minutes they get hard to work with so I just mix another batch using 1.5 cc each of resin and hardener. I make a few rods every year and usually cannot use up a 4oz. bottle before it goes bad so I don't worry about waste. The best tip I can give you is to use a heat gun on the finish after you apply it to a guide or wrap, this brings the air bubbles to the surface and helps the finish penetrate into the threads. The heat also softens the finish which will help you even it out if it was getting thick while being applied.
grey zone is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On

Forum Jump


All times are GMT -8. The time now is 01:51 AM.


Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2025, vBulletin Solutions Inc.
© 2002 Big Water's Edge. All rights reserved.